GaN nanoindentation: A micro-Raman spectroscopy study of local strain fields
Journal article   Peer reviewed

GaN nanoindentation: A micro-Raman spectroscopy study of local strain fields

Pascal Puech, François Demangeot, Jean Frandon, Claire Pinquier, Martin Kuball, Vladislav Domnich and Yury Gogotsi
Journal of applied physics, v 96(5), pp 2853-2856
Sep 2004