Logo image
Kink bands, nonlinear elasticity and nanoindentations in graphite
Journal article   Peer reviewed

Kink bands, nonlinear elasticity and nanoindentations in graphite

M. W BARSOUM, A MURUGAIAH, S. R KALIDINDI, T ZHEN and Y GOGOTSI
Carbon (New York), v 42(8-9), pp 1435-1445
2004

Abstract

Materials science Fullerenes and related materials; diamonds, graphite Specific materials Physics Cross-disciplinary physics: materials science; rheology Exact sciences and technology

Metrics

10 Record Views
150 citations in Scopus

Details

InCites Highlights

Data related to this publication, from InCites Benchmarking & Analytics tool:

Web of Science research areas
Chemistry, Physical
Materials Science, Multidisciplinary
Logo image