Journal article
Rapid Bonding of Ti3SiC2 and Ti3AlC2 by Pulsed Electrical Current Heating
Journal of the American Ceramic Society, v 97(12), pp 3721-3724
01 Dec 2014
Abstract
Inspired by pressure resistance welding of metallic materials, herein we describe how two MAX phasesTi(3)SiC(2) and Ti(3)AlC(2)were successfully joined by a rapid electric current heating method in a pulsed electric current sintering furnace. No welding agent was employed and the total processing time was less than 6min. When the bulk temperature of the joint couple exceeded 1070 degrees C, good joints, with shear strength above 50MPa, were achieved in both homo- and heterojunction joints.
Metrics
Details
- Title
- Rapid Bonding of Ti3SiC2 and Ti3AlC2 by Pulsed Electrical Current Heating
- Creators
- Lu Shen - Ningbo Institute of Industrial TechnologyJianming Xue - Peking UniversityMichel W. Barsoum - Drexel UniversityQing Huang - Ningbo Institute of Industrial Technology
- Publication Details
- Journal of the American Ceramic Society, v 97(12), pp 3721-3724
- Publisher
- Wiley
- Number of pages
- 4
- Resource Type
- Journal article
- Language
- English
- Academic Unit
- Materials Science and Engineering
- Web of Science ID
- WOS:000346099800002
- Scopus ID
- 2-s2.0-84915746912
- Other Identifier
- 991019167628504721
InCites Highlights
Data related to this publication, from InCites Benchmarking & Analytics tool:
- Collaboration types
- Domestic collaboration
- International collaboration
- Web of Science research areas
- Materials Science, Ceramics